LORE LAB Steel Test Database
No pass yet

No test of this steel has passed 600 cuts yet. The tests below show how close it has come.

4 tests so far.

Every test on one chart

4 tests, all shown
Passed (600 cuts) Failed (placed at the cut where it failed)

Micro-bevel angle (degrees per side)

Swipe the chart sideways to see the full angle range.

By brand

Each brand’s best result for this steel. Heat treat differs by brand, so the best passing angle can differ too.

Bestech
No pass yet · best attempt 200 cuts 4 tests

All tests

Every test for this steel, including heat damage, sorted by result and then angle. – means not recorded.

Notes
Failed 20° 10° 200 Bestech / VK-Void – Spruce
Failed 20° 15° 66 Bestech / VK-Void 59-60 Southern Pine
Failed 20° 15° 33 Bestech / VK-Void 59-60 Southern Pine
Failed 20° 10° 30 Bestech / VK-Void – Spruce
20° Failed 200 cuts
Brand
Bestech / VK-Void
Secondary bevel
10°
Hardness (HRC)
–
20° Failed 66 cuts
Brand
Bestech / VK-Void
Secondary bevel
15°
Hardness (HRC)
59-60
20° Failed 33 cuts
Brand
Bestech / VK-Void
Secondary bevel
15°
Hardness (HRC)
59-60
20° Failed 30 cuts
Brand
Bestech / VK-Void
Secondary bevel
10°
Hardness (HRC)
–