LORE LAB Steel Test Database
No pass yet

No test of this steel has passed 600 cuts yet. The tests below show how close it has come.

2 tests so far.

Every test on one chart

2 tests, all shown
Passed (600 cuts) Failed (placed at the cut where it failed)

Micro-bevel angle (degrees per side)

Swipe the chart sideways to see the full angle range.

By brand

Each brand’s best result for this steel. Heat treat differs by brand, so the best passing angle can differ too.

NERFY WU
No pass yet · best attempt 237 cuts 2 tests

All tests

Every test for this steel, including heat damage, sorted by result and then angle. – means not recorded.

Notes
Failed 15° 11° 8 NERFY WU – Spruce
Failed 20° 12° 237 NERFY WU – Spruce inconclusive
15° Failed 8 cuts
Brand
NERFY WU
Secondary bevel
11°
Hardness (HRC)
–
20° Failed 237 cuts
Brand
NERFY WU
Secondary bevel
12°
Hardness (HRC)
–
Notes
inconclusive