No pass yet
No test of this steel has passed 600 cuts yet. The tests below show how close it has come.
1 test so far.
Every test on one chart
1 test, all shown
Passed (600 cuts)
Failed (placed at the cut where it failed)
By brand
Each brand’s best result for this steel. Heat treat differs by brand, so the best passing angle can differ too.
Cold Steel
No pass yet · best attempt 24 cuts
1 test
All tests
Every test for this steel, including heat damage, sorted by result and then angle. – means not recorded.
| Notes | |||||||
|---|---|---|---|---|---|---|---|
| Failed | 24° | 13° | 24 | Cold Steel / PILLAR | – | Spruce |
24°
Failed
24 cuts
- Brand
- Cold Steel / PILLAR
- Secondary bevel
- 13°
- Hardness (HRC)
- –